Mates,
Please help. My PQR done was failed in hardness and impact test.
Details was
API-X60 Pipe(P1,Gr2)-16 inch Dia, 23mm Thick
Flange - A707 CL3 L5,(Not included in ASME sec 9 material grouping),16 inch Dia, 23mm Thick
GTAW-ER70S-2 -ROOT PASS & HOT PASS
SMAW-E7018-FILLING & CAP
CODE B31.8
NO PWHT Because as per code above 32mm only requires PWHT
PREHEAT done is 150 degress C,
It was passed in bend test and Tesile test... In Impact test test it passed with -18 C for parent metal (Flange&Pipe), Weld metal (SMAW), HAZ(SMAW & GTAW)but it failed on Weld metal (GTAW)
Please ask on your expertise advise.
Thank you
Please help. My PQR done was failed in hardness and impact test.
Details was
API-X60 Pipe(P1,Gr2)-16 inch Dia, 23mm Thick
Flange - A707 CL3 L5,(Not included in ASME sec 9 material grouping),16 inch Dia, 23mm Thick
GTAW-ER70S-2 -ROOT PASS & HOT PASS
SMAW-E7018-FILLING & CAP
CODE B31.8
NO PWHT Because as per code above 32mm only requires PWHT
PREHEAT done is 150 degress C,
It was passed in bend test and Tesile test... In Impact test test it passed with -18 C for parent metal (Flange&Pipe), Weld metal (SMAW), HAZ(SMAW & GTAW)but it failed on Weld metal (GTAW)
Please ask on your expertise advise.
Thank you