Hello,
We have cold-rolled ASTM A1011 SS GR33 powdercoated by an outside vendor. Recent review of our inventory shows that the powdercoating is blistering off of the metal and after scraping the powdercoating off there is red rust underneath. Some of these blisters look like round droplets of water.
The initial reaction is that the metal was rusty before the powdercoating process. Is it possible that this failure could be due to poor pretreatment of the metal during the coating process?
I'm not familiar enough with the coating process to know, and want to educate myself before I contact the vendor directly.
We have cold-rolled ASTM A1011 SS GR33 powdercoated by an outside vendor. Recent review of our inventory shows that the powdercoating is blistering off of the metal and after scraping the powdercoating off there is red rust underneath. Some of these blisters look like round droplets of water.
The initial reaction is that the metal was rusty before the powdercoating process. Is it possible that this failure could be due to poor pretreatment of the metal during the coating process?
I'm not familiar enough with the coating process to know, and want to educate myself before I contact the vendor directly.