Hello, All:

I would appreciate any suggestion for a potting/encapsulating compound to use in a device we are constructing.

The device is custom electromagnet used on an aircraft. The potting/encapsulating compound will fill the voids around the coil and it will not be required to offer any mechanical support to the device.

The material must operate up to 25,000 feet and withstand -40C to 150 C.

Thank you for the help,

Mac

 
We use Epoxylite #813-9 on a signal coil that is in a high fuel vapor area. High temperature
It is made for electronics applications.
epoxylite and PD George companies are suppliers and if this isn't sufficient, I'm sure they can recommend something that is.
 