Sep 2, 2010 #1 NotToScale Industrial Joined Jun 4, 2009 Messages 5 Location US Can anyone please advise what materials should be used in a component seal for that?
Sep 2, 2010 1 #2 flexibox Mechanical Joined Jun 23, 2007 Messages 343 Location AU Parker recommends EPDM for elastomers. 316S/S is good for wetted parts and Silicon Carbide Vs Carbon will be good, so a stanndard cartridge seals should be goood for this application. Upvote 0 Downvote
Parker recommends EPDM for elastomers. 316S/S is good for wetted parts and Silicon Carbide Vs Carbon will be good, so a stanndard cartridge seals should be goood for this application.
Sep 3, 2010 Thread starter #3 NotToScale Industrial Joined Jun 4, 2009 Messages 5 Location US Thank you, Flexibox. Upvote 0 Downvote