Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

post weld heat treatment of SS304L cladded vessel

Status
Not open for further replies.

212197

Mechanical
Joined
Jun 2, 2007
Messages
124
Location
IN
I have a requirement of vessel of SA 516 Gr 70+ ss304L CLADDING.
Vessel requires PWHT.


I am aware that to avoid sensitization, pwht cycle of ss cladded vessel is such that soaking temperature is reduced & soaking time is increased. (soaking temp 510 degree cel. Soaking time 10 hours/inch)

But now due to low carbon grade of SS i.e. ss304L, can I follow the soaking time & temp as UCS-56 cycle ?

i.e. I want to have pwht at 610 degree cel with time as per UCS-56.

 