We have a problem about our Diesel Engine type MAK 453 A and MAK 453 C, in the last few years we dont use water treatment for our cooling water, consequently the engine can't perform, cooling water leak to combustion chamber due to cylinder head crack, engine over temperatur and cant achieve the peak load due to cooling water poor heat transfer
Our laboratory check result for cooling water:
Conductivity : 186.6 Ms/cm
Total Dissolve Solid (TDS) : 93.46 ppm
PH : 7.22
Turbidity : 6.14 NTU
Total Suspended Solid (TSS): 10 mg/l
Anyone can help us about this diesel engine type cooling water requirement? We want to compare with the real standard cooling water for diesel engine (With source is better)
Big thanks
Our laboratory check result for cooling water:
Conductivity : 186.6 Ms/cm
Total Dissolve Solid (TDS) : 93.46 ppm
PH : 7.22
Turbidity : 6.14 NTU
Total Suspended Solid (TSS): 10 mg/l
Anyone can help us about this diesel engine type cooling water requirement? We want to compare with the real standard cooling water for diesel engine (With source is better)