Dec 3, 2009 #1 shalomw Materials Joined Dec 3, 2009 Messages 4 Location IL Hi I am looking for a polymer with high sensitivity (solubility) to Acetone vapor I have tried several photoresist compounds , some are better than others , but I would like to know if there are any even better one's. Thanks
Hi I am looking for a polymer with high sensitivity (solubility) to Acetone vapor I have tried several photoresist compounds , some are better than others , but I would like to know if there are any even better one's. Thanks
Dec 3, 2009 #2 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US You might want to look at Cellulose Acetate in the form of fiber, film, or molded parts. Upvote 0 Downvote
Dec 6, 2009 Thread starter #3 shalomw Materials Joined Dec 3, 2009 Messages 4 Location IL Thanks, The point is I have already tried quite a few polymers. I feel like I'm walking in the dark. I would really like to find some handbook info (or something similar) that compares different polymers with respect to their acetone sensitivity. Upvote 0 Downvote
Thanks, The point is I have already tried quite a few polymers. I feel like I'm walking in the dark. I would really like to find some handbook info (or something similar) that compares different polymers with respect to their acetone sensitivity.