Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Polyimide

Status
Not open for further replies.

proEdj

Mechanical
Joined
Dec 6, 2004
Messages
25
I have seen quite a wide range of Elastic Modulus values for polyimide pwb boards. Does anyone know of a reliable source that I can utilize to do a vibration analysis on a printed circuit board.

Thanks
 
PROEDJ: What is that you want to do? By vibration analysis do you mean a test like MIL-STD 810 or a resonance search or something else?

Regards
Dave
 
I was hoping to do a Pro-Mechanica or Ansys FEA analysis to determine the mode shapes and resonant frequencies of a board. I will also back this up with a hand calculation of the natural frequency. Both of these task require the Elastic Modulus, poisson's ratio, and density. I would actually prefer to have the properties of fully constructed printed circuit board.
 
Why not measure it? If the variances are that high, only a measurement will nail it down.