I have a 20"x20"x1" thick plywood panel that is connected to a 3/4" plywood skirt. (6)-6 GA screws are connecting the two pieces of assembly (screw tip is 1/2 into the 3/4" thick skirt. What is the screw design value for single shear connection, and what is the plywood-to-plywood shear capacity (is there a table in the NDS showing the plywood crushing capacity?). See attachment for description of the connection.

thank you in advance for the responses.
 
Replies continue below

Recommended for you

NDS (2001) Table 11.3.2B gives the dowel bearing strengths and specific gravity for Structural Panels. Table 11L gives some wood screws shear values. But, I would not accept this connection as it has only 1/2" embedment into the main (3/4" ply) member.