drawoh
Mechanical
- Oct 1, 2002
- 8,969
Our inspector has rejected some parts with 8-32UNC helical thread inserts located 1.4 to 1.7mm out of position. He has just asked me if these holes can be plugged an re-tapped. The material is aluminium 6061-T6.
Does anybody know how strong holes are when they are plugged and re-tapped?
--
JHG
Does anybody know how strong holes are when they are plugged and re-tapped?
--