The chemistry is as follows:
Carbon 0.05
Sulfur 0.004
Silicon 0.08
Manganese 0.10
Iron 19.3
Chromium 21.5
Molybdenum 2.79
Copper 0.01
Aluminum 0.25
Titanium 3.53
Cobalt 12.7
Nickel Matrix

The chemistry is of a 1.5" stud from a large turbine case.

Any help would be greatly appreciated.
 
I am looking for a source for Refractaloy 26 raw material in order to make some turbine studs, so if you found someone selling it, please let me know.
 
Check with several independent steam turbine repair contractors on the East coast and in the Midwest region. These folks have sources to obtain Refractaloy 26.
 