Please advise the suitability of Nickel Aluminium Bronze as pump material with monel shaft for fire water service using sea water
 
First, Go to the web site for the Ni Institute and look up publications on seawater pumps.
In general yes, this a combination of materials that would be used in ambient temperature seawater. There are other (more modern) options.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Check if this seawater is close to some other water bodies laden with trace quantities of corrosive chemicals. Material of construction may also be influenced by choice of biocide and mode of dosing (hypochlorite or copper sulphate generator etc).
 
This is an existing fire water pump at offshore. Thanks for the suggestions
 