What would the correct and cost effective process be for plating a sheet steel electrical panel? The panel has to conduct on all surfaces.

My local plater says "Zinc Plate with Blue Chromate" finish.

Any suggestions/experience?
 
We do Clear Zinc Plate (Yellow Chromate) and have had good results so far (~10 yrs.) Copper, Nickle, Nickle over Copper, etc. are all good depending on cost.
 
This is a panel to which other components will be mounted?

Typically such panels are finished with an insulating varnish or dielectric paint to make them non-conductive. This reduces the possibility of a short-to-ground if a terminal becomes lose, or some conductive debris enters the panel.

If you want a conductive panel then the suggested zinc would probably be ok, as would tin or electroless nickel.
 
Thanks for the help guys!

The panel will will have pem studs for mounting din rail and various components will mount via the din rail.

I will do a zinc/chromate finish. I will do more homework with this information.
 