Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

plastics 3

Status
Not open for further replies.

210269

Automotive
Joined
Apr 29, 2003
Messages
5
Location
GB
Is there a cost effective plastic /acrylic in manufacture that when used as clear glazing or partition in a vehicle that can meet all EU testing, ie abration strength ect.I Know of a material called Lexan from an American company but this is very costly.
 
Lexan® is the GE Plastics trademark for polycarbonate. This is used commonly for applications like yours. Other companies produce polycarbonate - try Calibre® from Dow and Apec®, Makrolon® and Makrofol® from Bayer. Websites for these companies are:







Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Acrylic is much better to abrasion than normal polycarbonate, and somewhat less expensive.

It is sometimes known by the trade names, Perspex, Plexiglass, Shinkolite or Oroglass.

It has a brittle type break, which might be a problem.

PC can be had with a treatment to improve it's scratch resistance, but that is even more expensive