Need vendors that actually have designed strand dryer for predrying strands before they enter the pelletizer . Tired of home made
 
When I ask Google for hits on "polymer strand drier" I get hits for machines that do that.


There is not any memory with less satisfaction than the memory of some temptation we resisted.
- James Branch Cabell
 
We simply lift the strands out of the water bath while they are still very hot and blow air across them with a few fans before the pelletiser, then blow more air over them while on the separator.

We adjust the bars that lift the strands so the pellets go into the bag at 70 to 80 deg C.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
We ran the still hot strand over thin metals tubes with holes in them so that the compressed air was able to blow air on the strands and dry them so no special machine required.


There is not any memory with less satisfaction than the memory of some temptation we resisted.
- James Branch Cabell
 