Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Plain Concrete Manhole Cover 1

Status
Not open for further replies.

john1525

Structural
Nov 24, 2009
10
I need to determine the plain concrete strength of an existing 4" thick 24" diameter concrete tank cover in flexure due to a 500 lbs load at the center. Chapter 22 commentary (R22.2.2) indicates that plain concrete should be limited to members that are primarily in a state of compression. However, section 22.5 provides the nominal moment strength of plain concrete. Is it acceptable to use equation 22.5 to determine its strength?

Any suggestions will be appreciated
 
Replies continue below

Recommended for you

For a concentrate load on the center, wouldn't be shear more critical? Yes, you can use criteria developed for structural plain concrete, but remember to check both shear & flexural.
 
Section 22.2 limits you. You can't use plain concrete for a flexural member with air under it.

 
I have to admit my mistake. Thank JAE for pointing out.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor