Does anyone have data or thoughts on the pitting performance of Type 304 stainless steel versus Type 304L?
Are they expected to be similar, or is one significantly different?
 
Replies continue below

Recommended for you

x-posting is not allowecd here. Please do not post the same thing in multiple fourms. Most of the people who read this fourm also read the stainless steel fourm.
 
In my opinion 304 and 304L have the same pitting behaviour, the L version has only better weldability properties due to its lower carbon content.
Regards
Massimo
 