hi,

We are doing type 2 sulfuric acid anodizing . We are facing pitting corrosion surfacing on aluminium plate on cathode with lead lining all along both the sides of the anodizing bath tub for quite some time now.

And it is growing day by day thus reducing the overall efficency .Can any body suggest some biocide to remove it without causing any side effect on aluminium surface .