Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Piping Material Selection for 37% HCL- cPVC, uPVC, PVC vs epoxy lined MS Piping

Status
Not open for further replies.

WarriorofGondolin

Mechanical
Joined
May 12, 2023
Messages
4
Location
BD
Hello Everyone,
I am working at a chemical plant that stores 37% conc. HCL in a double layered epoxy coated Carbon Steel tank and transfers that acid into dilution tanks via epoxy lined MS Piping. Due to ageing, we are planning on replacing the current tanks with FRP tanks and associated transfer piping with "cPVC, uPVC, or PVC". Pipe sizes are NPS 3 inch.
I have searched for chemical compatibility datasheet in the internet and found out that cPVC serves this purpose best.
Can anyone suggest some expert opinion on this matter as to the isolation valve material requirements and best piping materials?
 
Screenshot_2023-09-21_115232_aosx4v.png


= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
How long did the original tank and piping last?
Why is this change of materials?

DHURJATI SEN
Kolkata, India


 


Hello, the original HCL tank and associated transfer piping have been in operation for more than 25 years now. Tank epoxy re-coating was done 10 years back.
Decision to Change the materials of the tanks and piping was taken as the tank was no longer safe and leak-proof and the piping system was severely corroded at some places. Thank you.
 
Surely the identical material would run for another 25 years, the service and operating conditions remaining the same.

So why this material upgradation?

DHURJATI SEN
Kolkata, India


 
Thank you Pierreick. Sorry, it has been some time since I logged in.
I have gone through the pdfs. Certainly gave me some insight.
 