Feb 8, 2002 #1 ipung Mechanical Joined Jan 28, 2002 Messages 1 Location ID As we know that to corrosion prevention on burried pipe line, we can use bitumeus wraping. Could anyone advice what is the purpose of nylon reinforce in the bitumen layer for ? Regards
As we know that to corrosion prevention on burried pipe line, we can use bitumeus wraping. Could anyone advice what is the purpose of nylon reinforce in the bitumen layer for ? Regards
Feb 16, 2002 #2 DeltaCascade Chemical Joined Sep 27, 2001 Messages 241 Location CA To reinforce it? So it won't tear when handling and installing etc? Wayne// Upvote 0 Downvote