we have a control valve at which water enters at temperature 140 c and pressure 10 bars , after the control valve causes pressure drop flashing occurs in a pipe that is 2 meters long , the pipe material is of class C3D (carbon steel)of 100 mm so do we leave the pipe as it is short or upgrade the material and which material shall we use ?
 
Where does the 2 meter pipe go to? Where does it (the flashing condensate (?) end up at?

Draw a sketch of your problem.
 
Why do you think carbon steel is the incorrect material?

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Hi Adam001,

It depends... To better answer to your question give us more details. You may end up either (a) changing your process (pressure and temperature) and avoid flashing altogether, or (b) changing your material to P11 or P22 grade, or (c) changing (increasing) diameter of your pipe to mitigate damage done high velocities, or combination of all.

Thanks,
Curtis
 
What's the properties of the water, especially pH and dissolved oxygen?

Good luck,
Latexman

To a ChE, the glass is always full - 1/2 air and 1/2 water.
 