Frank1344
Mechanical
- Apr 25, 2005
- 133
Hello Friends,
We've got 24", ERW pipes which were manufactured by Cold Expanding.
Now the Bending Company is saying that they can not Guarantee that the Bends are going to have the same Yield Strength as the Parent Pipe does.
I want to get some ideas and comments about the subject before going to discuss it with the company.
I really appreciate the help.
Frank
We've got 24", ERW pipes which were manufactured by Cold Expanding.
Now the Bending Company is saying that they can not Guarantee that the Bends are going to have the same Yield Strength as the Parent Pipe does.
I want to get some ideas and comments about the subject before going to discuss it with the company.
I really appreciate the help.
Frank