You don't provide very much detail. Are you using prepregs and wet peel-ply? Is the pitting in the fabric weave openings, or are you working with uni-tape. Your problem could be air entrapment, excessive resin bleed, too high a volatile content, excessive resin bleed, and/or wrong cure cycle/bagging procedure.