Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Piezo material properties for ANSYS

Status
Not open for further replies.

vidiii

Industrial
Nov 13, 2006
36
Hi,
In ANSYS you can import material properties of piezo ceramics. But where can I find the specific material properties that are required by ANSYS?

You can find all kind of piezoelectric material properties on the net, like:

or


however, those are not compatible with what ANSYS requires. Where can I find the data that ANSYS requires?

The data that ANSYS needs:
! Material properties for PZT-4
!
mp,DENS,1,7700 ! Density, kg/m**3

tb,DPER,1 ! Relative permittivity at constant strain
tbdata,1,729,635,729
! - Alternative input of permittivity if used with SOLID5
! mp,PERX,1,729
! mp,PERY,1,635
! mp,PERZ,1,729
!
tb,ANEL,1 ! Anisotropic elastic stiffness, N/m^2
tbdata,1,13.9E10,7.43E10,7.78E10 ! c11,c13,c12
tbdata,7,11.5E10,7.43E10 ! c33,c13
tbdata,12,13.9E10 ! c11
tbdata,16,2.56E10 ! c44
tbdata,19,2.56E10 ! c44
tbdata,21,3.06E10 ! c66

tb,PIEZ,1 ! Piezoelectric stress coefficients, C/m^2
tbdata,2,-5.2 ! e31
tbdata,5,15.1 ! e33
tbdata,8,-5.2 ! e31
tbdata,10,12.7 ! e15
tbdata,15,12.7 ! e15
 