Sep 22, 2003 #1 mcdm Electrical Joined Sep 4, 2002 Messages 21 Location GB i have heard that because of the explosive nature in some paint and oil plants, some tools i.e. spanners are made of phosphor bronze can anyone offer advice on where i can get any information? best regards mcdm
i have heard that because of the explosive nature in some paint and oil plants, some tools i.e. spanners are made of phosphor bronze can anyone offer advice on where i can get any information? best regards mcdm
Sep 22, 2003 1 #2 patprimmer New member Joined Nov 1, 2002 Messages 13,816 Location US Tool suppliers to the underground mineing industry, especially coal mines, can supply such tools. Do a google search on hand tools mineing, and choose one who can supply in your area, wherever that might be Regards pat Upvote 0 Downvote