After internal inspection of an exchanger, seat for jacketed gasket was reported corroded, as a consequence of this the sealing area was reducid 50% in the worst area.
There is a tolerance about what is the percentage of lost seat acceptable?
 
Replies continue below

Recommended for you

Hello Joss,

See PCC-1 appendix D. You can purchase the standard for $92.00 US from ASME

 