Hi everybody. I have a question. Is there a standard for material FR-4? And does it exist a standardized designation for this material with foil thickness and etc?
 
Replies continue below

Recommended for you

FR-4 is a grade designation, not a material description... big difference between the two.

The foil thickness is whatever is offered by the manufacturer of one specific instance of FR-4, but most manufacturers create 1/8-, 1/4-, 1/2-, 3/4-, 1-, and 2-ounce copper on various core thicknesses. They'll also do custom thicknesses, but expect to pay for thousands of panels worth at a time.

Dan - Owner
Footwell%20Animation%20Tiny.gif
 
In case you're wondering about the "ounce" unit of measure, it's explained nicely here: PCB Universe
 