I have a cylinder in UNS S31803, approx 33.5" O/D, 25" I/D, 18" long, weighing about 840kg. There is a requirement to have it passivated in accordance with ASTM A380 section A2.

Can anybody suggest a UK supplier who might be able to do the work?

Thanks.
 
Find someone that does pharma fabrication. I'll look in my notes when I get back to the office. There are a few.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
No guarantees but you might want to contact Porstmouth Aviation (google should find it), they have a reasonable treatment facility and do some fairly large stuff though I don't remember them passivating anything that big when I was there.

KENAT,

Have you reminded yourself of faq731-376 recently, or taken a look at posting policies: What is Engineering anyway: faq1088-1484
 
Kenat,

I tried Portsmouth Aviation, who can do the size but not the weight. The same was true of a number of others, but I eventually found Anopol. I'm now waiting hopefully for a quote to come back.
 