Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Parts to build a thermoforming machine

Status
Not open for further replies.

crix

Mechanical
May 14, 2002
8
Hi

Can you give me a break down of the specific parts that would be necessary to construct a fairly small thermoforming machine employing a vacuum? Cost is an important factor and clearity of description of the parts is most wanted.
Also what are they types of plastics most commonly used with the above process?

Thanks.
 
Replies continue below

Recommended for you

I previously answered your question about home brew thermoforming device.

Now: To materials.

High impact polystyrene is most used. It forms readily, is available in sheet form from many suppliers in many thicknesses. Fairly cheap.

ABS is also used. Not quite as avaiable, more costly.

Polycarbonate is much more difficult to form, much more costly.

I suggest high imact polystyrene.

 