Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Partial pressure of CO2 measurement

Status
Not open for further replies.

SukhpalSingh

Petroleum
Joined
May 19, 2016
Messages
25
Location
IQ
I need to run an experiment for CO2 corosion measurement and I need to do this with different values of partial pressure of CO2. therfore, I will appreciate any help about what the equations and the instruments that I need to use for this purpose.
 
Will there be any H2S involved? I presume not.

We would use a blended gas. Say if the highest fraction that we wanted was 20% CO2 in N2, we would buy a mix at 40%. Then it is just pressure regulators and gauges. If the test is not static (but with flowing gas) then you also need flow meters.
You could do it from pure gases but that is more difficult to get correct.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Thank you for your reply, actually I will used a pure gas with continous flow since it is available for me rather than the mixture. therefore, if that possible can you expalin steps and measurements involved in this situation.
 