Corrosion and subsequent failure of unbounded PT tendons due to the use of salt to deice used to be a big problem in northern parking garages, but that was a long time ago.
 
They did get something like 5" of rain that night. Maybe a flat spot on the top deck?
 
Maybe a plugged drain if water collection was enough.
 
Hmmmm...are those temporary guardrails/barricades? Could there have been work going on up there prior to the collapse?
 
There were already barricades around a portion of the parkade when it collapsed
(Google Maps for reference, also here)


Screenshot_at_2023-08-25_12-22-48_ituzd6.jpg


Screenshot_at_2023-08-25_12-23-19_p8mk4o.jpg


Barriers_h43296.jpg

cleveland.com
 
yeah - and shoring on the level below. So they knew there was a problem, but perhaps underestimated the scope or severity. Sounds a little too familiar...
 
Criminal overtones (cleveland.com)

cleveland.com said:
In December 2021, the city of Willowick charged Shoregate Towers NS, LLC, with a host of criminal misdemeanors in Willoughby Municipal Court related to property maintenance violations.

How does it work that you get to plead no contest only to appeal?
 
You can file anytime you like, but you might never plead.
 
cleveland19.com

Suggestions of lightning strike causing damage and car fire as well as a resident claiming that I-beams were being replaced to address rust.
 