Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Paraffin Wax Actuator Design guide???

Status
Not open for further replies.

quizzical1

Mechanical
Jul 6, 2004
180
Hi All,

Does anyone know of a good reference book on designing these type of thermal actuators?
I know S. Vernet from his early patents showed examples back in the 1930's - 1950's but was wondering if anyone ever came across a design guide.

TIA

~Q
 
Replies continue below

Recommended for you

They are pretty simple - you need to determine the volumetric expansion of wax for the temperature required and figure out how much pressure the external load of actuation will be produced plus the load of the return spring. Other than that it's just a small hydraulic device that has a solid-liquid transition for the working fluid.
 
The Vernet company still exists, you can google for them. They have a pretty decent engineering department that can help you out.

FWIW...an electric motor actuator will usually be more efficient than a wax actuator if you are operating at near room temperature (i.e. you apply electrical heating to make the motion you want). Reason being that the motor can move to a position and hold it (with suitable non-slip gearing), but the wax pellet requires constant thermal input to hold a position other than its "cold" position. Places where wax motors work well is in thermal regulation, where operating temperatures are within melting range of wax/oil mixtures.
 