Apr 16, 2004 #1 rfulky Mechanical Joined Feb 11, 2003 Messages 11 Location US Is there a coating that can be used on studs to keep paint and e-coat off the threads without using a stud protector?
Is there a coating that can be used on studs to keep paint and e-coat off the threads without using a stud protector?
Apr 17, 2004 #2 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US Fluorocarbon masking is used routinely for this purpose. Try Nylok: http://www.nylok.com Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
Fluorocarbon masking is used routinely for this purpose. Try Nylok: http://www.nylok.com Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
Jul 25, 2004 #3 Chr1s Automotive Joined Apr 12, 2002 Messages 30 Location US Teflon - We use it on weld studs in the body shop prior to E-coat and paint. Sometimes it also pays to add a nut with paint cutter threads. Upvote 0 Downvote
Teflon - We use it on weld studs in the body shop prior to E-coat and paint. Sometimes it also pays to add a nut with paint cutter threads.