Nov 22, 2010 #1 Sjaak2010 Materials Joined Nov 8, 2010 Messages 1 Location NL Can anybody help me with the P-number for P92/F92 material. I've got a dated ASME BPVC which doesn't show the P-number for this alloy. Thanks
Can anybody help me with the P-number for P92/F92 material. I've got a dated ASME BPVC which doesn't show the P-number for this alloy. Thanks
Nov 22, 2010 1 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US There has been no specific P-No assigned because this material is permitted by Code Case only. If it is used in Code Case 2179-7, the material shall be considered as P-No 15E, Group 1. Upvote 0 Downvote
There has been no specific P-No assigned because this material is permitted by Code Case only. If it is used in Code Case 2179-7, the material shall be considered as P-No 15E, Group 1.