P92/F92 P-number 1

Status
Not open for further replies.

Sjaak2010

Materials
Nov 8, 2010
1
Can anybody help me with the P-number for P92/F92 material. I've got a dated ASME BPVC which doesn't show the P-number for this alloy. Thanks
 
Replies continue below

Recommended for you

There has been no specific P-No assigned because this material is permitted by Code Case only. If it is used in Code Case 2179-7, the material shall be considered as P-No 15E, Group 1.
 