After i remove the cap`s, my intention it´s cut off the HAZ of the P91 base metal, re-weld for the final components, PWHT and perform a hardness test. These welds will be Golden welds. My question is: following this procedure which will be the better choice for the welding material: P91, P22 or CS?
If i choose the P91, and PWHT i will be behind the Tcrit. of the CS, and my affraid it´s the damage that i can input to the CS Cap, and have problems when i expose that material to 2500psig(Hidro test Pressure).
If i choose CS welding material and PWHT with the temperatur of the CS, i will have the P91 side with a value of hardness for outside the máximum admisible value.
Your comments it will highly appreciated.