We have a 1.813" M.W bottle header ( Existing ) P4A

Welding to a 1.75" M.W new bottle header spool piece ( New ) P5A


My question is - Obviously we go with the higher material grade for the PWHT procedure ( P5A ) , but should I also use the bigger thickness ( 1.813" instead of 1.750" ) for my soak time ? ( 1:45 mins as opposed to 2 hours ) I know this is a negligable amount of time but I was wondering for future reference should it involve thicker sections.



Thank you very much in advance
 
Replies continue below

Recommended for you

Almost always, you must use the thicker section when two sections are being welded and then PWHT'ed.

I'm hedging my answer there, but I can think of no exceptions to that rule.
 
First and foremost, READ the code of construction for what defines nominal thickness for PWHT.
 
The term "nominal thickness" as used in Tables PW-39-1 through PW39-14 is defined as follows :

(A) For full penetration butt welds , the nominal thickness is the thinner of the parts being joined.




It was looking me right in the face under the P1 PWHT table. Thanks for the direction metengr
 
Sure, since I belong to Section I standards committee. I need to assist others.
 
we want to weld pipes P1+P5B, P1+P5A, P4+P5A, P4+P15E, P5A+P15E what electrodes to be used for TIG welding and SMAW and PWHT requirements.
P1=SA106-B or C, P4= SA335P11, P5A=SA335P22, A182F22, P5B A217C5, P15E=A182F91, A335P91,A217C12A. Can anybody help
Thank you
 
What is nominal thickness if both the full penetration butt welded parts(thickness 1.5") are of same thickness according to UW-40(f)(1).??
Does it need PWHT if its P.NO-1????
 