Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

P-No of SA-612

Status
Not open for further replies.

David403

Petroleum
May 15, 2006
7
Is there any one has the experience of SA-612?
For VIII-1 P-No is 10C
But for VIII-2, P-No is 1
Any one can explain it?
 
Replies continue below

Recommended for you

What? No such thing. P-No's assigned in Section II Table I are what they are and P-No's cannot change for the same material.
 
2007 ASME Section II Part D Table 5A shows a P-number of 1 for SA-612. It's probably a typographical error.
 
Section II-D Table 5A shows P-No1 for SA-612
We are first time to use this table.
Should assume this is a typographical error.
 
David

I would look at a previous version to see if this is a typographical error.

If it is, TGS4 provided this helpful information in another thread:

Interesting observation. The appropriate way to address an "error" like that is to send an e-mail to the secretary of the Codes and Standards committee. The contact info is on this web page
Please let us know the resolution to your issue.

Note that any other responses that you might receive on eng-tips would be only anonymous opinions and worth, well, what you pay for them. There is only one adequate resolution, and that is the one that I stated above.

Patricia Lougheed

Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of the Eng-Tips Forums.
 
Status