What is the test pressures of hoses for axy-acety welding and what is the minimum length and diameters of the hoses to be used?
 
Replies continue below

Recommended for you

Hi there cemcayan,
Saw your question and popped to the w/shop-I have pipes there with a 10mm(3/8")inside diameter 12metres in legnth
with a test pressure of 20bar(around 280psi)
Legnth and bore sizes should be to your personal preference.
However-strongly suggest Flasback Arresters!
Good luck
TWWeld.
 