Good morning guys, hope all of you are well. Just thought I post in here to see if anybody has the information i am looking for. I am looking for the maximum allowable thickness of the chrome layer on the CROMAX IH 482 from OVAKO. And also the amount of microcracks per mm^2.

Thanks for the help guys, have a great Friday!!!
 
Replies continue below

Recommended for you

You will need to contact Ovako directly for this information. The Cr thickness will likely be in the range of 20-30 micrometers. Crack density should be in the range of 50-150 cracks/mm.
 