One of our customers require that we don't break the edge prior to F.P.I on a hole therefore we must drill a burr less hole??? I came across Orbital drilling but have yet have enough information to use has anyone done it?
 
Replies continue below

Recommended for you

No matter which way you cut it you will still have a burr, but I think that if you use the orbital drilling it will produce a much smaller burr