5
I am in a situation where I have a 40mm thick piece of Acrylic between two polarizers. My problem is that the acrylic turns birefringent at around 35 deg C, and optical performance is badly degraded. I have contacted Ineos about Perspex, but it is not available in the right thickness in the US. DOes anyone know of a material with similar optical performance (>90% transmissivity, ~1.5 refractive index, with superior thermal characterisitcs.

Thanks
Andy
 
Replies continue below

Recommended for you

Try ATOHAAS North America Inc 800 523 1532 or 215 785 8290.

Other possibilities: Cyro Industries 203 795 6081

ICI Acrylics 800 386 2175

Good Luck


 
Why you do not take e.g. from the company BULKHEAD to glass in Mainz. With plastics you have always the problem with the high thermal expansion.
Sincerely
Heinz Federau
federau@web.de
 
Try TOPAS from TICONA. It is a cyclo-olefinic copolymer with excellent optics and a high glass transition temperature and a low thermal expansion, so I assume this would solve your birefringence problems.
 