onshore Pipe line, that will be carrying Gas +Condensate well fluid from an on shore well pad to the Gas oil separation plant. The length of pipe line is approx. 40 km. underground portion of which is made of sour rated and externally 3 LPE coated carbon Steel . Above ground portion of the pipe line where the well pad is connected is made of SS 316 L and is externally hot insulated. Well fluid (gas + condensate)carries H2S of 6 to 8 Mole %, CO2 of 10 mole % and water of approx. 25 mole %. Temperature of well fluid is around 80 deg C and pressure = 100 bar. The Chloride level in the produced (formation) water is around 150,000 ppm.
i am evaluating this study for its damage mechanism. list of damage mechanism that susceptible for this study are :
1)H2S cracking
2)HIC
3)CL SCC
4)Corrosion Erosion
my suggestion are as follow :
for buried pipeline - to change its material to super duplex material n control its CP to -850mV to -450mV.
any comments on the study?
i am evaluating this study for its damage mechanism. list of damage mechanism that susceptible for this study are :
1)H2S cracking
2)HIC
3)CL SCC
4)Corrosion Erosion
my suggestion are as follow :
for buried pipeline - to change its material to super duplex material n control its CP to -850mV to -450mV.