Old steel shed certification

Status
Not open for further replies.

PowerRanger

Structural
Jan 17, 2005
60
Hi fellows

A question about old steel shed certification. How can I find out the steel capacity under corrosion.

Thank you.
 
Replies continue below

Recommended for you

If corrosion is significant, determine the residual section and calculate capacity. This would require removal of the corrosion (possibly by sandblasting) and measuring the thickness etc of the elements.
If the corrosion is not much more than surface rust it could be ignored I think.

A question like this which is not directly related to an AS could be posted in the 'structural eng other topics' forum eg, where you would get a lot more replies.

John
 