I'm thinking of using Oilon plastic as a bearing material in a subsea application but can't find any consistent information on its' water absorbtion rate. Data sheets I've found on line have values ranging from 0% to 6.2%, does anyone have reliable information as to what the rate actually is?
Thanks for any help.
Pete
 
Replies continue below

Recommended for you

Oilon is a cast nylon 6 - it will absorb water.

You would be better using a lubricated acetal - either with silicon based oil or PTFE.

H

www.tynevalleyplastics.co.uk

It's ok to soar like an eagle, but weasels don't get sucked into jet engines.
 
Thanks Pud, I'll have a look for some of that.