I have some problem for O-ring seal.
It used under condition syntetic oil and high temperature.I found it like a mud or soming like that.
my quesion is what happen ?
 
Replies continue below

Recommended for you

What grade of o' ring are you using, grade of oil and temperature? EPDM will disintergrate very quickly in oil. Viton can be used up to 180 Deg C max. Above that you will require Kalrez or Isolast.
 
I agree with DonBallantyne, it sounds like a compatability problem with the fluid and o-ring material.
 
you can also visit simrit.com and find some tools about how to choose the proper material and design a adequate groove for your application. The small "mud" particles are burned oil parts "thanks" to very high tepmerature or an inadequate oil-quality or just simple dirth according to poorly flitered oil in the system.

 
Soory!! That I too late to reply.
I used it for Gas Turbine, material is Viton ,Temperatur about 180 C.
 
Viton will deteriorate because of alcohol based liquids.
 
Use a PTFE based seal with an metal spring energizer. PTFE is compatible with most chemical and has higher service temperature, up to 450F.
 
FEP (teflon encapsulated Viton) is better & cheeper solution for your problem