O-ring as an extension spring?

Status
Not open for further replies.

Glenn Gordon

Mechanical
Jan 29, 2018
10
Hello,

I have an application where I would like to use an o-ring as an extension spring.

It is not a heavy duty application and it is not subject to any cyclical loading.

This o-ring in this mechanism is to hold tension between two pins whose center to center distance are infrequently adjusted.

Can you recommend what o-ring material would offer the best longevity in this application?

Thanks,
Glenn




 
Replies continue below

Recommended for you

That would depend on the environmental conditions.

John R. Baker, P.E. (ret)
EX-Product 'Evangelist'
Irvine, CA
Siemens PLM:
UG/NX Museum:

The secret of life is not finding someone to live with
It's finding someone you can't live without
 
The o-ring is in contact with two stainless pins and the ambient air (room temperature).

Glenn
 
If you look at the ASTM D 2000 and/or SAE J200 spec for rubber there are a few materials that have ultimate elongation as high as 600%. Given the minimal stated requirements, one of these would be "best". However, I suspect in this case the "best" would be whatever the local building supply has on hand.

----------------------------------------

The Help for this program was created in Windows Help format, which depends on a feature that isn't included in this version of Windows.
 
Nitrile would probably work fine too, and be a bit cheaper than epdm. It would also relax less (maintain a more constant tension over time). But, epdm will stand up to a lot more stuff (ozone, uv) that might be coming through your "ambient air". We use a "bungee cord" to hold a lid on a product that sits in a potentially ozone filled, potentially moist environment, we fabricate the cord from some 1/8" epdm cord stock.
 