balven
Materials
- Aug 29, 2011
- 9
Hi all,
For duplex stainlees steel flanged joints, we had specified ASTM A453 Gr. 660 bolts and ASTM A194 Gr. 2HM nuts (as per API 6A). However, we propose to change the nuts to a corrosion-resistant alloy (CRA) material. Can someone let me know any CRA material grades for nuts that are compatible with Gr. 660 bolts ? The main concern here is galling. Can we use nuts to A453 Gr. 660 (same grade as bolts)?
Would appreciate if you could share your experiences/observations on CRA nuts on Gr. 660 bolts.
Thanks,
Balvendra Pal
For duplex stainlees steel flanged joints, we had specified ASTM A453 Gr. 660 bolts and ASTM A194 Gr. 2HM nuts (as per API 6A). However, we propose to change the nuts to a corrosion-resistant alloy (CRA) material. Can someone let me know any CRA material grades for nuts that are compatible with Gr. 660 bolts ? The main concern here is galling. Can we use nuts to A453 Gr. 660 (same grade as bolts)?
Would appreciate if you could share your experiences/observations on CRA nuts on Gr. 660 bolts.
Thanks,
Balvendra Pal