As you know, for groove area an increase or decrease > 25% in number of passes needs prequalification.
I want to know Where the number of passes mention in WPS?


Regards
H.Mirhosseini
 
Correct post
As you know, for groove area an increase or decrease > 25% in number of passes needs requalification.
I want to know Where the number of passes mention in WPS?


Regards
H.Mirhosseini
 
With the 2004 edition of AWS D1.1, this requirement for requalification has been dropped.
As to where the pases are shown, see the examples in Annex E of the Code. The pass count should either show up in the sketch and/or listed in the table if there are variations between passes. The PQR must show more information regarding pass data, than a WPS might need.
 