Is it permitted more then one longitudinal welds in one shell according to ASME Section VIII Div 2?
 
Replies continue below

Recommended for you

Thank you Steve,
Yes I mean cylindrical shell section using more than one plate.
 
Just remember to stagger the seams if more than one shell section.
 